Effects of la content on the properties of Ba1-xLa xTiO3 powders prepared by spray pyrolysis

D. S. Jung, H. Y. Koo, H. C. Jang, Yun Chan Kang

Research output: Contribution to journalArticle

12 Citations (Scopus)

Abstract

Nano-sized Bai1-xLaxTiO3 (0 < x < 0.03) powders were prepared by ultrasonic spray pyrolysis from the spray solution with citric acid. The mean sizes of the primary particles decreased from 110 nm to 59 nm when the x of the Ba1-xLaxTiO 3 powders was changed from 0 to 0.03. The BET surface areas of the powders changed from 9.1 m2/g to 16.9 m2/g. The pure BaTiO3 and La-doped BaTiO3 powders had both tetragonal and cubic crystal structures. The average grain size of the sintered BaTiO 3 specimen was 2.8 uμrn, while those of the La-doped BaTiO 3 pellets ranged from 1.04 uμm to 0.68 uμm according to the doping concentrations of La. The dielectric constant of Ba1-xLa xTiO3(0.01 <x< 0.03) pellets ranged from 2500 to 3855 when sintered at 1280°

Original languageEnglish
Pages (from-to)809-814
Number of pages6
JournalMetals and Materials International
Volume15
Issue number5
DOIs
Publication statusPublished - 2009 Oct 1
Externally publishedYes

Fingerprint

Spray pyrolysis
Powders
pyrolysis
sprayers
pellets
citric acid
Citric acid
Citric Acid
Permittivity
ultrasonics
Crystal structure
grain size
Ultrasonics
Doping (additives)
permittivity
crystal structure

Keywords

  • Barium titanate
  • Nano powder
  • Spray pyrolysis

ASJC Scopus subject areas

  • Condensed Matter Physics
  • Mechanics of Materials
  • Metals and Alloys
  • Materials Chemistry

Cite this

Effects of la content on the properties of Ba1-xLa xTiO3 powders prepared by spray pyrolysis. / Jung, D. S.; Koo, H. Y.; Jang, H. C.; Kang, Yun Chan.

In: Metals and Materials International, Vol. 15, No. 5, 01.10.2009, p. 809-814.

Research output: Contribution to journalArticle

@article{1ab037fa8f8540ba8808333db9b2e127,
title = "Effects of la content on the properties of Ba1-xLa xTiO3 powders prepared by spray pyrolysis",
abstract = "Nano-sized Bai1-xLaxTiO3 (0 < x < 0.03) powders were prepared by ultrasonic spray pyrolysis from the spray solution with citric acid. The mean sizes of the primary particles decreased from 110 nm to 59 nm when the x of the Ba1-xLaxTiO 3 powders was changed from 0 to 0.03. The BET surface areas of the powders changed from 9.1 m2/g to 16.9 m2/g. The pure BaTiO3 and La-doped BaTiO3 powders had both tetragonal and cubic crystal structures. The average grain size of the sintered BaTiO 3 specimen was 2.8 uμrn, while those of the La-doped BaTiO 3 pellets ranged from 1.04 uμm to 0.68 uμm according to the doping concentrations of La. The dielectric constant of Ba1-xLa xTiO3(0.01",
keywords = "Barium titanate, Nano powder, Spray pyrolysis",
author = "Jung, {D. S.} and Koo, {H. Y.} and Jang, {H. C.} and Kang, {Yun Chan}",
year = "2009",
month = "10",
day = "1",
doi = "10.1007/s12540-009-0809-2",
language = "English",
volume = "15",
pages = "809--814",
journal = "Metals and Materials International",
issn = "1598-9623",
publisher = "Korean Institute of Metals and Materials",
number = "5",

}

TY - JOUR

T1 - Effects of la content on the properties of Ba1-xLa xTiO3 powders prepared by spray pyrolysis

AU - Jung, D. S.

AU - Koo, H. Y.

AU - Jang, H. C.

AU - Kang, Yun Chan

PY - 2009/10/1

Y1 - 2009/10/1

N2 - Nano-sized Bai1-xLaxTiO3 (0 < x < 0.03) powders were prepared by ultrasonic spray pyrolysis from the spray solution with citric acid. The mean sizes of the primary particles decreased from 110 nm to 59 nm when the x of the Ba1-xLaxTiO 3 powders was changed from 0 to 0.03. The BET surface areas of the powders changed from 9.1 m2/g to 16.9 m2/g. The pure BaTiO3 and La-doped BaTiO3 powders had both tetragonal and cubic crystal structures. The average grain size of the sintered BaTiO 3 specimen was 2.8 uμrn, while those of the La-doped BaTiO 3 pellets ranged from 1.04 uμm to 0.68 uμm according to the doping concentrations of La. The dielectric constant of Ba1-xLa xTiO3(0.01

AB - Nano-sized Bai1-xLaxTiO3 (0 < x < 0.03) powders were prepared by ultrasonic spray pyrolysis from the spray solution with citric acid. The mean sizes of the primary particles decreased from 110 nm to 59 nm when the x of the Ba1-xLaxTiO 3 powders was changed from 0 to 0.03. The BET surface areas of the powders changed from 9.1 m2/g to 16.9 m2/g. The pure BaTiO3 and La-doped BaTiO3 powders had both tetragonal and cubic crystal structures. The average grain size of the sintered BaTiO 3 specimen was 2.8 uμrn, while those of the La-doped BaTiO 3 pellets ranged from 1.04 uμm to 0.68 uμm according to the doping concentrations of La. The dielectric constant of Ba1-xLa xTiO3(0.01

KW - Barium titanate

KW - Nano powder

KW - Spray pyrolysis

UR - http://www.scopus.com/inward/record.url?scp=70450263546&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=70450263546&partnerID=8YFLogxK

U2 - 10.1007/s12540-009-0809-2

DO - 10.1007/s12540-009-0809-2

M3 - Article

AN - SCOPUS:70450263546

VL - 15

SP - 809

EP - 814

JO - Metals and Materials International

JF - Metals and Materials International

SN - 1598-9623

IS - 5

ER -