Abstract

The formation process and microwave dielectric properties of the Mg 2V2O7 ceramics were investigated. The MgV 2O6 phase that was formed at around 450°C interacted with remnant MgO above 590°C to form a homogeneous monoclinic Mg 2V2O7 phase. Finally, this monoclinic Mg 2V2O7 phase was changed to a triclinic Mg 2V2O7 phase for the specimen fired at 800°C. Sintering at 950°C for more than 5 h produced high-density triclinic Mg2V2O7 ceramics. In particular, the Mg2V2O7 ceramics sintered at 950°C for 10 h exhibited the good microwave dielectric properties of εr=10.5, Q × f=58 275 GHz, and τf=-26.9 ppm/°C.

Original languageEnglish
Pages (from-to)1621-1624
Number of pages4
JournalJournal of the American Ceramic Society
Volume92
Issue number7
DOIs
Publication statusPublished - 2009 Jul 1

Fingerprint

dielectric property
ceramics
Dielectric properties
Microwaves
Sintering
microwave

ASJC Scopus subject areas

  • Ceramics and Composites
  • Materials Chemistry

Cite this

Formation and microwave dielectric properties of the Mg2V 2O7 Ceramics. / Joung, Mi Ri; Kim, Jin Seong; Song, Myung Eun; Nahm, Sahn; Paik, Jong Hoo; Choi, Byung Hyun.

In: Journal of the American Ceramic Society, Vol. 92, No. 7, 01.07.2009, p. 1621-1624.

Research output: Contribution to journalArticle

Joung, Mi Ri ; Kim, Jin Seong ; Song, Myung Eun ; Nahm, Sahn ; Paik, Jong Hoo ; Choi, Byung Hyun. / Formation and microwave dielectric properties of the Mg2V 2O7 Ceramics. In: Journal of the American Ceramic Society. 2009 ; Vol. 92, No. 7. pp. 1621-1624.
@article{d05ba9f88c654c48a2d45240a681e56c,
title = "Formation and microwave dielectric properties of the Mg2V 2O7 Ceramics",
abstract = "The formation process and microwave dielectric properties of the Mg 2V2O7 ceramics were investigated. The MgV 2O6 phase that was formed at around 450°C interacted with remnant MgO above 590°C to form a homogeneous monoclinic Mg 2V2O7 phase. Finally, this monoclinic Mg 2V2O7 phase was changed to a triclinic Mg 2V2O7 phase for the specimen fired at 800°C. Sintering at 950°C for more than 5 h produced high-density triclinic Mg2V2O7 ceramics. In particular, the Mg2V2O7 ceramics sintered at 950°C for 10 h exhibited the good microwave dielectric properties of εr=10.5, Q × f=58 275 GHz, and τf=-26.9 ppm/°C.",
author = "Joung, {Mi Ri} and Kim, {Jin Seong} and Song, {Myung Eun} and Sahn Nahm and Paik, {Jong Hoo} and Choi, {Byung Hyun}",
year = "2009",
month = "7",
day = "1",
doi = "10.1111/j.1551-2916.2009.03078.x",
language = "English",
volume = "92",
pages = "1621--1624",
journal = "Journal of the American Ceramic Society",
issn = "0002-7820",
publisher = "Wiley-Blackwell",
number = "7",

}

TY - JOUR

T1 - Formation and microwave dielectric properties of the Mg2V 2O7 Ceramics

AU - Joung, Mi Ri

AU - Kim, Jin Seong

AU - Song, Myung Eun

AU - Nahm, Sahn

AU - Paik, Jong Hoo

AU - Choi, Byung Hyun

PY - 2009/7/1

Y1 - 2009/7/1

N2 - The formation process and microwave dielectric properties of the Mg 2V2O7 ceramics were investigated. The MgV 2O6 phase that was formed at around 450°C interacted with remnant MgO above 590°C to form a homogeneous monoclinic Mg 2V2O7 phase. Finally, this monoclinic Mg 2V2O7 phase was changed to a triclinic Mg 2V2O7 phase for the specimen fired at 800°C. Sintering at 950°C for more than 5 h produced high-density triclinic Mg2V2O7 ceramics. In particular, the Mg2V2O7 ceramics sintered at 950°C for 10 h exhibited the good microwave dielectric properties of εr=10.5, Q × f=58 275 GHz, and τf=-26.9 ppm/°C.

AB - The formation process and microwave dielectric properties of the Mg 2V2O7 ceramics were investigated. The MgV 2O6 phase that was formed at around 450°C interacted with remnant MgO above 590°C to form a homogeneous monoclinic Mg 2V2O7 phase. Finally, this monoclinic Mg 2V2O7 phase was changed to a triclinic Mg 2V2O7 phase for the specimen fired at 800°C. Sintering at 950°C for more than 5 h produced high-density triclinic Mg2V2O7 ceramics. In particular, the Mg2V2O7 ceramics sintered at 950°C for 10 h exhibited the good microwave dielectric properties of εr=10.5, Q × f=58 275 GHz, and τf=-26.9 ppm/°C.

UR - http://www.scopus.com/inward/record.url?scp=67650080711&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=67650080711&partnerID=8YFLogxK

U2 - 10.1111/j.1551-2916.2009.03078.x

DO - 10.1111/j.1551-2916.2009.03078.x

M3 - Article

VL - 92

SP - 1621

EP - 1624

JO - Journal of the American Ceramic Society

JF - Journal of the American Ceramic Society

SN - 0002-7820

IS - 7

ER -