Microwave dielectric properties of (Zn1-xMnx) 2P2O7

Jian Jiang Bian, Dong-Wan Kim, Kugsun Hong

Research output: Contribution to journalArticle

6 Citations (Scopus)

Abstract

The microwave dielectric properties of (Zn1-xMn x)2P2O7 was investigated. It was observed that the pure α-(Zn2P2O7 exhibits a rapid shrinkage above 700 °C and reaches the shrinkage of about 16% at 875 °C. It was shown that for Mn2P2O 7, rapid shrinkage occurs above the temperature of about 900 °C and reaches the shrinkage of about 14% at 1000 °C. It was found that the dielectric constant of the solid solution increases firstly and then decreases with the increase of Mn2P2O7 addition.

Original languageEnglish
Pages (from-to)1801-1803
Number of pages3
JournalJournal of Materials Science
Volume40
Issue number7
DOIs
Publication statusPublished - 2005 Apr 1
Externally publishedYes

Fingerprint

shrinkage
Dielectric properties
dielectric properties
Microwaves
microwaves
Solid solutions
Permittivity
solid solutions
permittivity
Temperature
temperature

ASJC Scopus subject areas

  • Materials Science(all)
  • Electronic, Optical and Magnetic Materials
  • Condensed Matter Physics

Cite this

Microwave dielectric properties of (Zn1-xMnx) 2P2O7 . / Bian, Jian Jiang; Kim, Dong-Wan; Hong, Kugsun.

In: Journal of Materials Science, Vol. 40, No. 7, 01.04.2005, p. 1801-1803.

Research output: Contribution to journalArticle

Bian, Jian Jiang ; Kim, Dong-Wan ; Hong, Kugsun. / Microwave dielectric properties of (Zn1-xMnx) 2P2O7 In: Journal of Materials Science. 2005 ; Vol. 40, No. 7. pp. 1801-1803.
@article{c02690f47d924499bbf86d824604368e,
title = "Microwave dielectric properties of (Zn1-xMnx) 2P2O7",
abstract = "The microwave dielectric properties of (Zn1-xMn x)2P2O7 was investigated. It was observed that the pure α-(Zn2P2O7 exhibits a rapid shrinkage above 700 °C and reaches the shrinkage of about 16{\%} at 875 °C. It was shown that for Mn2P2O 7, rapid shrinkage occurs above the temperature of about 900 °C and reaches the shrinkage of about 14{\%} at 1000 °C. It was found that the dielectric constant of the solid solution increases firstly and then decreases with the increase of Mn2P2O7 addition.",
author = "Bian, {Jian Jiang} and Dong-Wan Kim and Kugsun Hong",
year = "2005",
month = "4",
day = "1",
doi = "10.1007/s10853-005-0698-4",
language = "English",
volume = "40",
pages = "1801--1803",
journal = "Journal of Materials Science",
issn = "0022-2461",
publisher = "Springer Netherlands",
number = "7",

}

TY - JOUR

T1 - Microwave dielectric properties of (Zn1-xMnx) 2P2O7

AU - Bian, Jian Jiang

AU - Kim, Dong-Wan

AU - Hong, Kugsun

PY - 2005/4/1

Y1 - 2005/4/1

N2 - The microwave dielectric properties of (Zn1-xMn x)2P2O7 was investigated. It was observed that the pure α-(Zn2P2O7 exhibits a rapid shrinkage above 700 °C and reaches the shrinkage of about 16% at 875 °C. It was shown that for Mn2P2O 7, rapid shrinkage occurs above the temperature of about 900 °C and reaches the shrinkage of about 14% at 1000 °C. It was found that the dielectric constant of the solid solution increases firstly and then decreases with the increase of Mn2P2O7 addition.

AB - The microwave dielectric properties of (Zn1-xMn x)2P2O7 was investigated. It was observed that the pure α-(Zn2P2O7 exhibits a rapid shrinkage above 700 °C and reaches the shrinkage of about 16% at 875 °C. It was shown that for Mn2P2O 7, rapid shrinkage occurs above the temperature of about 900 °C and reaches the shrinkage of about 14% at 1000 °C. It was found that the dielectric constant of the solid solution increases firstly and then decreases with the increase of Mn2P2O7 addition.

UR - http://www.scopus.com/inward/record.url?scp=27544442707&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=27544442707&partnerID=8YFLogxK

U2 - 10.1007/s10853-005-0698-4

DO - 10.1007/s10853-005-0698-4

M3 - Article

AN - SCOPUS:27544442707

VL - 40

SP - 1801

EP - 1803

JO - Journal of Materials Science

JF - Journal of Materials Science

SN - 0022-2461

IS - 7

ER -