Abstract

ZnO/Ag composite particles for contact materials were prepared from colloidal solutions by ultrasonic spray pyrolysis. The colloidal solutions were prepared by adding unagglomerated nanometer ZnO particles into the silver nitrate solutions. The composite particles were not hollow, and had spherical morphology with a uniform dispersion of nanometer ZnO particles inside the Ag matrix. The nanometer ZnO particles were completely coated with silver by heterogeneous precipitation onto the preexisting ZnO particles. The weight ratio of ZnO to Ag in the composite particles was varied from 0.08 to 0.33 by changing the amount of nanometer ZnO particles in the colloidal solutions. The mean size of the ZnO/Ag composite particles were increased from 0.85 to 1.24 μm as the weight ratio of ZnO to Ag increased from 0.08 to 0.33.

Original languageEnglish
Pages (from-to)129-133
Number of pages5
JournalMaterials Letters
Volume40
Issue number3
DOIs
Publication statusPublished - 1999 Jan 1
Externally publishedYes

Fingerprint

Zinc Oxide
Spray pyrolysis
Zinc oxide
Silver
zinc oxides
pyrolysis
sprayers
silver
preparation
Composite materials
Silver Nitrate
composite materials
Contacts (fluid mechanics)
Nitrates
Ultrasonics
silver nitrates
electric contacts
hollow
ultrasonics

ASJC Scopus subject areas

  • Materials Science(all)
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Cite this

Preparation of zinc oxide-dispersed silver particles by spray pyrolysis of colloidal solution. / Kang, Yun Chan; Park, S. B.

In: Materials Letters, Vol. 40, No. 3, 01.01.1999, p. 129-133.

Research output: Contribution to journalArticle

@article{15537686a2604dcb841e536b0191460f,
title = "Preparation of zinc oxide-dispersed silver particles by spray pyrolysis of colloidal solution",
abstract = "ZnO/Ag composite particles for contact materials were prepared from colloidal solutions by ultrasonic spray pyrolysis. The colloidal solutions were prepared by adding unagglomerated nanometer ZnO particles into the silver nitrate solutions. The composite particles were not hollow, and had spherical morphology with a uniform dispersion of nanometer ZnO particles inside the Ag matrix. The nanometer ZnO particles were completely coated with silver by heterogeneous precipitation onto the preexisting ZnO particles. The weight ratio of ZnO to Ag in the composite particles was varied from 0.08 to 0.33 by changing the amount of nanometer ZnO particles in the colloidal solutions. The mean size of the ZnO/Ag composite particles were increased from 0.85 to 1.24 μm as the weight ratio of ZnO to Ag increased from 0.08 to 0.33.",
author = "Kang, {Yun Chan} and Park, {S. B.}",
year = "1999",
month = "1",
day = "1",
doi = "10.1016/S0167-577X(99)00061-0",
language = "English",
volume = "40",
pages = "129--133",
journal = "Materials Letters",
issn = "0167-577X",
publisher = "Elsevier",
number = "3",

}

TY - JOUR

T1 - Preparation of zinc oxide-dispersed silver particles by spray pyrolysis of colloidal solution

AU - Kang, Yun Chan

AU - Park, S. B.

PY - 1999/1/1

Y1 - 1999/1/1

N2 - ZnO/Ag composite particles for contact materials were prepared from colloidal solutions by ultrasonic spray pyrolysis. The colloidal solutions were prepared by adding unagglomerated nanometer ZnO particles into the silver nitrate solutions. The composite particles were not hollow, and had spherical morphology with a uniform dispersion of nanometer ZnO particles inside the Ag matrix. The nanometer ZnO particles were completely coated with silver by heterogeneous precipitation onto the preexisting ZnO particles. The weight ratio of ZnO to Ag in the composite particles was varied from 0.08 to 0.33 by changing the amount of nanometer ZnO particles in the colloidal solutions. The mean size of the ZnO/Ag composite particles were increased from 0.85 to 1.24 μm as the weight ratio of ZnO to Ag increased from 0.08 to 0.33.

AB - ZnO/Ag composite particles for contact materials were prepared from colloidal solutions by ultrasonic spray pyrolysis. The colloidal solutions were prepared by adding unagglomerated nanometer ZnO particles into the silver nitrate solutions. The composite particles were not hollow, and had spherical morphology with a uniform dispersion of nanometer ZnO particles inside the Ag matrix. The nanometer ZnO particles were completely coated with silver by heterogeneous precipitation onto the preexisting ZnO particles. The weight ratio of ZnO to Ag in the composite particles was varied from 0.08 to 0.33 by changing the amount of nanometer ZnO particles in the colloidal solutions. The mean size of the ZnO/Ag composite particles were increased from 0.85 to 1.24 μm as the weight ratio of ZnO to Ag increased from 0.08 to 0.33.

UR - http://www.scopus.com/inward/record.url?scp=0032672937&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0032672937&partnerID=8YFLogxK

U2 - 10.1016/S0167-577X(99)00061-0

DO - 10.1016/S0167-577X(99)00061-0

M3 - Article

AN - SCOPUS:0032672937

VL - 40

SP - 129

EP - 133

JO - Materials Letters

JF - Materials Letters

SN - 0167-577X

IS - 3

ER -