Spherical shape BaNd2Ti5O14 (BNT) powders were prepared by post-treatment of the precursor powders obtained by spray pyrolysis. The mean size and geometric standard deviation of the powders prepared at a low flow rate of the carrier gas as 5 Lmin-1 were 0.73μm and 1.30. The powders post-treated at a temperature of 1000°C had a single phase of BNT without impurity peaks. The BNT powders had similar compositions to that of the spray solution. Necking between the powders occurred at a sintering temperature of 1100°C. The BNT powders with spherical shape changed to the rod-like crystals after sintering at temperatures above 1200°C. The aspect ratio of the rod-like crystals increased with increasing the sintering temperatures.

Original languageEnglish
Pages (from-to)1289-1294
Number of pages6
JournalJournal of the Ceramic Society of Japan
Volume116
Issue number1360
DOIs
Publication statusPublished - 2008 Jan 1
Externally publishedYes

Fingerprint

Spray pyrolysis
Powders
pyrolysis
sprayers
sintering
Sintering
rods
Temperature
Crystals
temperature
crystals
aspect ratio
Aspect ratio
standard deviation
flow velocity
Gases
Flow rate
Impurities
impurities
Chemical analysis

Keywords

  • Dielectric material
  • Spray pyrolysis
  • Titanate

ASJC Scopus subject areas

  • Ceramics and Composites
  • Chemistry(all)
  • Condensed Matter Physics
  • Materials Chemistry

Cite this

Spherical shape BaNd2Ti5O14 powders prepared by spray pyrolysis. / Han, Jin Man; Jung, Dae Soo; Cho, Jung Sang; Kang, Yun Chan.

In: Journal of the Ceramic Society of Japan, Vol. 116, No. 1360, 01.01.2008, p. 1289-1294.

Research output: Contribution to journalArticle

Han, Jin Man ; Jung, Dae Soo ; Cho, Jung Sang ; Kang, Yun Chan. / Spherical shape BaNd2Ti5O14 powders prepared by spray pyrolysis. In: Journal of the Ceramic Society of Japan. 2008 ; Vol. 116, No. 1360. pp. 1289-1294.
@article{b6dba61147e84b24b9030da22271476b,
title = "Spherical shape BaNd2Ti5O14 powders prepared by spray pyrolysis",
abstract = "Spherical shape BaNd2Ti5O14 (BNT) powders were prepared by post-treatment of the precursor powders obtained by spray pyrolysis. The mean size and geometric standard deviation of the powders prepared at a low flow rate of the carrier gas as 5 Lmin-1 were 0.73μm and 1.30. The powders post-treated at a temperature of 1000°C had a single phase of BNT without impurity peaks. The BNT powders had similar compositions to that of the spray solution. Necking between the powders occurred at a sintering temperature of 1100°C. The BNT powders with spherical shape changed to the rod-like crystals after sintering at temperatures above 1200°C. The aspect ratio of the rod-like crystals increased with increasing the sintering temperatures.",
keywords = "Dielectric material, Spray pyrolysis, Titanate",
author = "Han, {Jin Man} and Jung, {Dae Soo} and Cho, {Jung Sang} and Kang, {Yun Chan}",
year = "2008",
month = "1",
day = "1",
doi = "10.2109/jcersj2.116.1289",
language = "English",
volume = "116",
pages = "1289--1294",
journal = "Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan",
issn = "1882-0743",
publisher = "Ceramic Society of Japan/Nippon Seramikkusu Kyokai",
number = "1360",

}

TY - JOUR

T1 - Spherical shape BaNd2Ti5O14 powders prepared by spray pyrolysis

AU - Han, Jin Man

AU - Jung, Dae Soo

AU - Cho, Jung Sang

AU - Kang, Yun Chan

PY - 2008/1/1

Y1 - 2008/1/1

N2 - Spherical shape BaNd2Ti5O14 (BNT) powders were prepared by post-treatment of the precursor powders obtained by spray pyrolysis. The mean size and geometric standard deviation of the powders prepared at a low flow rate of the carrier gas as 5 Lmin-1 were 0.73μm and 1.30. The powders post-treated at a temperature of 1000°C had a single phase of BNT without impurity peaks. The BNT powders had similar compositions to that of the spray solution. Necking between the powders occurred at a sintering temperature of 1100°C. The BNT powders with spherical shape changed to the rod-like crystals after sintering at temperatures above 1200°C. The aspect ratio of the rod-like crystals increased with increasing the sintering temperatures.

AB - Spherical shape BaNd2Ti5O14 (BNT) powders were prepared by post-treatment of the precursor powders obtained by spray pyrolysis. The mean size and geometric standard deviation of the powders prepared at a low flow rate of the carrier gas as 5 Lmin-1 were 0.73μm and 1.30. The powders post-treated at a temperature of 1000°C had a single phase of BNT without impurity peaks. The BNT powders had similar compositions to that of the spray solution. Necking between the powders occurred at a sintering temperature of 1100°C. The BNT powders with spherical shape changed to the rod-like crystals after sintering at temperatures above 1200°C. The aspect ratio of the rod-like crystals increased with increasing the sintering temperatures.

KW - Dielectric material

KW - Spray pyrolysis

KW - Titanate

UR - http://www.scopus.com/inward/record.url?scp=57149136574&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=57149136574&partnerID=8YFLogxK

U2 - 10.2109/jcersj2.116.1289

DO - 10.2109/jcersj2.116.1289

M3 - Article

AN - SCOPUS:57149136574

VL - 116

SP - 1289

EP - 1294

JO - Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan

JF - Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan

SN - 1882-0743

IS - 1360

ER -