Use of LiCl flux in the preparation of Y2O3:Eu phosphor particles by spray pyrolysis

Yun Chan Kang, Hyun Sook Roh, Seung Bin Park, Hee Dong Park

Research output: Contribution to journalArticle

44 Citations (Scopus)

Abstract

The effect of LiCl flux on the luminescence characteristics, crystallinity and morphology of Y2O3:Eu phosphor particles was investigated. The maximum PL intensity of particles directly prepared at 1300 °C from solution with LiCl flux was 50% higher than that of particles prepared from solution without flux. The PL intensities of particles prepared at 700 and 900 °C from flux solution were 200 and 134% of those of particles prepared from solution without flux at the same preparation temperatures. Activation of Eu dopant was fully occurred even at 700 °C when LiCl flux was used while high temperature above 1100 °C was required without flux, LiCl flux played an important role of improving activation degree of Eu dopant into Y2O3 host and reducing defects of particles.

Original languageEnglish
Pages (from-to)1661-1665
Number of pages5
JournalJournal of the European Ceramic Society
Volume22
Issue number9-10
DOIs
Publication statusPublished - 2002 Sep 1
Externally publishedYes

Fingerprint

Spray pyrolysis
Phosphors
Fluxes
Chemical activation
Doping (additives)
Luminescence
Temperature
Defects

Keywords

  • Flux
  • LiCl flux
  • Phosphor
  • Photoluminescence
  • Spray pyrolysis
  • YO:Eu

ASJC Scopus subject areas

  • Ceramics and Composites

Cite this

Use of LiCl flux in the preparation of Y2O3:Eu phosphor particles by spray pyrolysis. / Kang, Yun Chan; Roh, Hyun Sook; Park, Seung Bin; Park, Hee Dong.

In: Journal of the European Ceramic Society, Vol. 22, No. 9-10, 01.09.2002, p. 1661-1665.

Research output: Contribution to journalArticle

Kang, Yun Chan ; Roh, Hyun Sook ; Park, Seung Bin ; Park, Hee Dong. / Use of LiCl flux in the preparation of Y2O3:Eu phosphor particles by spray pyrolysis. In: Journal of the European Ceramic Society. 2002 ; Vol. 22, No. 9-10. pp. 1661-1665.
@article{9dbeb3eae5ea471aa8aa3b239bd0b4f1,
title = "Use of LiCl flux in the preparation of Y2O3:Eu phosphor particles by spray pyrolysis",
abstract = "The effect of LiCl flux on the luminescence characteristics, crystallinity and morphology of Y2O3:Eu phosphor particles was investigated. The maximum PL intensity of particles directly prepared at 1300 °C from solution with LiCl flux was 50{\%} higher than that of particles prepared from solution without flux. The PL intensities of particles prepared at 700 and 900 °C from flux solution were 200 and 134{\%} of those of particles prepared from solution without flux at the same preparation temperatures. Activation of Eu dopant was fully occurred even at 700 °C when LiCl flux was used while high temperature above 1100 °C was required without flux, LiCl flux played an important role of improving activation degree of Eu dopant into Y2O3 host and reducing defects of particles.",
keywords = "Flux, LiCl flux, Phosphor, Photoluminescence, Spray pyrolysis, YO:Eu",
author = "Kang, {Yun Chan} and Roh, {Hyun Sook} and Park, {Seung Bin} and Park, {Hee Dong}",
year = "2002",
month = "9",
day = "1",
doi = "10.1016/S0955-2219(01)00462-9",
language = "English",
volume = "22",
pages = "1661--1665",
journal = "Journal of the European Ceramic Society",
issn = "0955-2219",
publisher = "Elsevier BV",
number = "9-10",

}

TY - JOUR

T1 - Use of LiCl flux in the preparation of Y2O3:Eu phosphor particles by spray pyrolysis

AU - Kang, Yun Chan

AU - Roh, Hyun Sook

AU - Park, Seung Bin

AU - Park, Hee Dong

PY - 2002/9/1

Y1 - 2002/9/1

N2 - The effect of LiCl flux on the luminescence characteristics, crystallinity and morphology of Y2O3:Eu phosphor particles was investigated. The maximum PL intensity of particles directly prepared at 1300 °C from solution with LiCl flux was 50% higher than that of particles prepared from solution without flux. The PL intensities of particles prepared at 700 and 900 °C from flux solution were 200 and 134% of those of particles prepared from solution without flux at the same preparation temperatures. Activation of Eu dopant was fully occurred even at 700 °C when LiCl flux was used while high temperature above 1100 °C was required without flux, LiCl flux played an important role of improving activation degree of Eu dopant into Y2O3 host and reducing defects of particles.

AB - The effect of LiCl flux on the luminescence characteristics, crystallinity and morphology of Y2O3:Eu phosphor particles was investigated. The maximum PL intensity of particles directly prepared at 1300 °C from solution with LiCl flux was 50% higher than that of particles prepared from solution without flux. The PL intensities of particles prepared at 700 and 900 °C from flux solution were 200 and 134% of those of particles prepared from solution without flux at the same preparation temperatures. Activation of Eu dopant was fully occurred even at 700 °C when LiCl flux was used while high temperature above 1100 °C was required without flux, LiCl flux played an important role of improving activation degree of Eu dopant into Y2O3 host and reducing defects of particles.

KW - Flux

KW - LiCl flux

KW - Phosphor

KW - Photoluminescence

KW - Spray pyrolysis

KW - YO:Eu

UR - http://www.scopus.com/inward/record.url?scp=0036722318&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=0036722318&partnerID=8YFLogxK

U2 - 10.1016/S0955-2219(01)00462-9

DO - 10.1016/S0955-2219(01)00462-9

M3 - Article

AN - SCOPUS:0036722318

VL - 22

SP - 1661

EP - 1665

JO - Journal of the European Ceramic Society

JF - Journal of the European Ceramic Society

SN - 0955-2219

IS - 9-10

ER -